GH3030 Superalloy Round Bar Manufacturer | Bright & Peeled Surface | In Stock for Sale

GH3030 Superalloy Round Bar Manufacturer | Bright & Peeled Surface | In Stock for Sale
GH3030 is a nickel-based solid solution strengthened superalloy bar (containing approximately 80% nickel and 20% chromium), renowned for its excellent oxidation resistance and high plasticity, making it ideal for operating environments below 800°C. This alloy is supplied in round bar form and is commonly used in aerospace components, gas turbine combustors, and high-temperature furnace components.
What is GH3030 material?
GH3030 is a high-temperature nickel-based superalloy primarily used in components requiring high oxidation resistance and thermal stability. Due to its excellent performance in high-temperature environments, GH3030 is widely used in the aerospace and power generation industries.

Top-grade GH3030 round bar specifications
As a leading supplier of nickel alloys, Gnee Steel's GH3030 high-temperature bars strictly comply with GB, GJB, and equivalent international standards. Our bars are meticulously designed to remain stable in extreme environments up to 800°C.
| Technical Feature | Details & Capabilities |
| Material Grade | GH3030 / Nickel Alloy 3030 / Nimonic 75 / EI435 (ЭИ435) |
| Diameter Range | Φ 6.0mm – Φ 250mm (Custom larger sizes available) |
| Tolerance Grades | h8, h9, h10 or customized precision tolerances |
| Surface Finish | Mirror-like Bright Ground, Precision Peeled, or Black Forged |
| Standard Compliance | GB/T 14992, GB/T 14994, GJB 2297 |
| Production Process | VIM (Vacuum Induction Melting) + ESR (Electroslag Remelting) |
| GH3030 Bar Chemical Composition and Mechanical properties |
| Grade | C | Mn | P | S | Si | Cr | Fe | Al | Ti | Cu |
| GH3030 | 0.12 max | 0.7 max | 0.03 max | 0.02 max | 0.8 max | 19.0 – 22.0 | 1.5 max | 0.15 max | 0.15 – 0.35 | 0.2 max |
| Element | Density (g/cm3) |
Melting Point (°C) |
Tensile Strength RM N/MM2 |
Elongation A5% |
| GH3030 | 8.4 | 1374-1420 | ≥ 590 | ≥ 35% |
Contact us now to get a quote for GH3030 round bars
Why choose to source GH3030 bars from Gnee Steel's high-temperature alloy plant?
In the highly competitive superalloy materials supply market, we stand out for our superior structural integrity and metallurgical purity.
Mirror-like finish: Our precision-ground GH3030 bars have a surface roughness Ra ≤ 0.8μm, perfect for high-speed automatic lathes.
Sufficient stock and fast lead times: We have standard sizes (Φ10, Φ20, Φ50, Φ80, Φ100mm) in stock to ensure your projects are completed on time.
Exceptional high-temperature strength: GH3030 bars retain high ductility and oxidation resistance, making them ideal for aero-engine shafts.
Quality certification: 100% ultrasonically tested (UT). Every order includes an EN 10204 3.1 factory test certificate (MTC).

Request GH3030 bar technical data sheet
Wide Applications of GH3030 Bar Stock
Our GH3030 high-temperature alloy bars are high-performance solutions for the following fields:
Aerospace and Defense: Aircraft engine shafts, support structures, and turbine components.
Industrial Fasteners: High-strength bolts, pins, and nuts capable of operating at 700-800°C.
Industrial Furnaces: Drive shafts, load-bearing hooks, and supports for heat treatment furnaces.
Petrochemicals: High-temperature valve stems and corrosion-resistant shafts.




Contact us now to get the latest export price for GH3030 in 2026

Stop paying exorbitant fees to middlemen. Procurement directly from reputable Chinese GH3030 high-temperature alloy round bar factories. Our technical sales team is ready to provide you with quick quotes and professional material consultation services.
Email: [ru@gneesteelgroup.com]
WhatsApp/WeChat: +86 15824687445
Website: [https://www.china-plate-steel.com/]
FAQ
Q: What are the international equivalent grades of GH3030 round bars?
A: GH3030 is equivalent to the Russian grade EI435 (ЭИ435) and the British grade Nimonic 75. It also conforms to Alloy 75 (UNS N06075) and W.Nr. 2.4951. Choosing our GH3030 bars allows you to obtain the same performance as these Western brands cost-effectively.
Q: Which surface finish is best suited for my application?
A:Bright finish (h8/h9): Best suited for CNC machining of small precision parts such as bolts.
Peeled finish (h10/h11): Suitable for general mechanical parts requiring removal of the outermost layer for defect detection.
Black finish: Best suited for customers planning secondary forging or hot working.
Q: Is GH3030 easy to machine?
A: GH3030 is a solid solution strengthened nickel-based alloy. While tougher than stainless steel, it offers better machinability compared to precipitation-hardening alloys such as GH4169. We recommend using carbide tools and reducing cutting speeds for optimal machining results.
Q: How do you guarantee the internal quality of large-diameter bars?
A: For forged bars (typically larger than Φ80mm), we use electroslag remelting (ESR) to ensure a uniform microstructure. We perform 100% ultrasonic testing (UT) to ensure the absence of internal porosity, cracks, or inclusions.
Q: Do you accept small trial orders?
A: Yes! As a customer-centric superalloy manufacturer, we accept small batch orders (starting from 20kg-50kg) of stock products so you can verify our product quality before bulk purchasing.