A comprehensive overview of AMS 5596 Inconel-718 alloy plates

A comprehensive overview of AMS 5596 Inconel-718 alloy plates
The AMS 5596 standard specifies Inconel 718 (Alloy 718), a high-strength, precipitation-hardened nickel-chromium alloy known for its excellent strength, corrosion resistance, and weldability across a wide range of temperatures, from cryogenic to high temperatures (strength up to 1300°F, oxidation resistance up to 1800°F). Therefore, it is crucial for aerospace applications (jet engines, rockets) and other demanding applications such as fasteners, rings, and cryogenic storage tanks. It combines high performance with ease of processing and effectively resists creep and post-weld cracking.
What are the disadvantages of Inconel 718?
Disadvantages of INCONEL 718 and alternative solutions
Despite its excellent mechanical properties and corrosion resistance, Inconel 718 also has some disadvantages: Cost: Due to its complex manufacturing process, Inconel 718 is expensive. Difficult to machine: Its high hardness makes material removal difficult and accelerates tool wear.

1. AMS 5596 Specification Overview: Core Requirements of an Aerospace Standard
AMS 5596 is an Aerospace Material Specification published by SAE International, specifically defining the chemical composition, physical, and mechanical property requirements for Inconel 718 alloy sheet, strip, and plate in the solution heat-treated and precipitation-hardened (aged) condition for use in welded structural components. This specification is an authoritative standard in the aerospace industry, representing the highest level of material quality and consistency assurance.
Key Certifications and Scope of Application:
Main Application Areas: Aerospace engine casings, mounting brackets, load-bearing structural components, combustion chamber parts, and other areas requiring high-strength welded structures.
Core Condition: The material is supplied in the solution heat-treated condition, facilitating subsequent forming and welding. Standard aging treatment must be performed after welding to achieve final performance.
Strict Traceability: Requires complete material heat number traceability and compliant material test reports (MTR/Certificate of Conformance).

Sample of AMS 5596 plate material standard (MTR) provided by GNEE
2. Comparison of AMS 5596 with common commercial specifications (such as ASTM B670)
For Inconel 718 sheet material, different standards specify different supply conditions and performance priorities.
| Comparison Dimension | AMS 5596 (Aerospace Specific) | Typical Commercial Specifications (e.g., ASTM B670 / ASME SB670) | Core Differences & Selection Significance |
|---|---|---|---|
| Core Objective | To ensure material for fusion welding or aerospace structures has optimal weldability and post-weld performance. | Covers a wider range of industrial applications, including oil & gas and general industry. | AMS 5596 has stricter and more specific requirements for welding suitability. |
| Typical Supply Condition | Solution Treated condition. The user performs aging treatment after welding. | Solution Treated & Aged condition or Solution Treated condition. | The AMS 5596 condition is optimized for subsequent welding processes; commercial plate can be used directly as high-strength components. |
| Heat Treatment Requirements | Specifies solution treatment temperature and cooling method (typically rapid cooling) to ensure grain size control and complete dissolution of phases. | Heat treatment requirements are relatively broad, possibly allowing wider parameter ranges. | AMS 5596 has stricter heat treatment controls, ensuring high consistency between batches. |
| Mechanical Property Requirements | Specifies a maximum hardness in the solution-treated condition (typically HRC ≤ 34) to ensure good cold formability and weldability. Final properties are achieved after post-weld aging. | Directly specifies minimum strength values in the aged condition (e.g., Tensile ≥ 1275 MPa). | AMS 5596 focuses on process adaptability; commercial specifications focus on final in-service performance. |
| Non-Destructive Testing (NDT) | Typically mandates Ultrasonic Testing (UT) to ensure the plate is free from internal defects that could affect welded structures. | UT is usually an additional agreement requirement, not mandatory. | AMS 5596 has higher acceptance criteria for internal material quality. |
| Documentation & Traceability | Requires complete test reports compliant with AMS specifications and traceable heat number information. | Provides a standard Material Test Report (MTR); traceability depends on customer agreement. | Quality assurance and traceability requirements are more stringent in the aerospace supply chain. |
3. Key performance data for AMS 5596 Inconel 718 sheet material
| element | Ni | Cr | Fe | Nb+Ta | Mo | Ti | Al | Co | C | Mn | Si | P | S | B | Cu |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| scope (%) | 50-55 | 17-21 | margin | 4.75-5.5 | 2.8-3.3 | 0.65-1.15 | 0.2-0.8 | ≤1.0 | ≤0.08 | ≤0.35 | ≤0.35 | ≤0.015 | ≤0.015 | ≤0.006 | ≤0.3 |
Typical Mechanical Properties (Solution-Treated Condition)
Hardness: HRC ≤ 34 (Typical value HRC 28-33), ensuring good machinability.
Tensile Strength: ~860-1035 MPa (Solution-treated condition)
Elongation: ≥ 25% (Solution-treated condition)
Post-Weld Aging Treatment and Final Properties
Standard Aging Process: 720°C ± 10°C / 8 hours, furnace cooling to 620°C ± 10°C / holding for 8 hours, then air cooling.
Typical Properties in Post-Weld Aged Condition:
Ultimate Tensile Strength: ≥ 1275 MPa
0.2% Yield Strength: ≥ 1035 MPa
Elongation: ≥ 12%
4. Processing and Welding Specific Guidelines
The processing of plates conforming to AMS 5596 specifications is primarily geared towards welding.
Welding Process Key Points
Welding Material Selection: The use of ERNiFeCr-2 welding wire conforming to AMS 5832 specifications or equivalent materials is recommended.
Welding Method: TIG (GTAW) is the preferred method, but plasma arc welding (PAW), electron beam welding (EBW), and laser beam welding (LBW) are also widely used.
Preheating and Interpass Temperature: Preheating is generally not required, but the interpass temperature should be controlled to ≤ 150°C to prevent hot cracking.
Post-Weld Treatment: The above-mentioned standard aging treatment must be performed to relieve welding residual stress and precipitate strengthening phases in the weld and heat-affected zone, achieving strength matching that of the base material.
Forming and Machining
Cold Forming: Excellent cold formability in the solution-treated state, allowing for bending, stretching, and other operations.
Hot Forming: Temperature range 1010°C - 1120°C; re-solution treatment is required after forming.
Machining: It is strongly recommended to complete all machining in the solution-treated state, followed by stress relief annealing (if necessary) before final aging. Machining in the aged state is extremely difficult.

Gnee AMS 5596 Inconel 718 sheet factory
SAE AMS 5596 Inconel 718 Plate Specification Scope
Before selecting Inconel 718 material for your next aerospace project, you need to understand the scope of the SAE AMS 5596 specification. SAE AMS 5596 specifies the requirements for corrosion-resistant and heat-resistant nickel alloys. These alloys come in various forms, such as plates, strips, foils, and sheets. This specification covers materials with a thickness of 1.00 inch (25.4 mm) or less. This means you can use Inconel 718 in many aerospace components requiring high performance and reliability.
You will frequently use Inconel 718 plates and strips because these forms offer flexibility in manufacturing and design. The specification sets clear limits on thickness and width, allowing you to select the appropriate material for your application. The table below shows the allowable ranges for Inconel 718 plates, strips, and related forms:
| Form | Thickness Range | Width Range |
|---|---|---|
| Inconel 718 sheet | 0.1 to 5 mm | 0.5 to 1 m |
| Alloy 718 plate | 2.5 to 100 mm | 0.5 to 2 m |
| ASTM B670 UNS N07718 coil | 0.1 to 5 mm | 0.5 to 1.2 m |
| Alloy Inconel 718 strips | 0.05 to 3 mm | 5 to 200 mm |
Please contact us to obtain the latest inventory list of AMS 5596 Inconel 718 alloy plates, complete certification documents, and free technical consultation on welding and post-weld heat treatment processes.

Gnee Steel is a professional manufacturer of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy industries, and we can provide customized alloy material solutions according to customer needs. For alloy material price inquiries or to request customized alloy material solutions, please feel free to contact us at ru@gneesteelgroup.com for a quote.