Standard & Classification
Standard: EN 10025 (2004) - Hot-rolled structural steel products
Type: Non-alloy or fine-grain steel (Parts 2-6 of EN 10025)
Key Grades:
S355JR (+20°C impact)
S355J0 (0°C impact)
S355J2 (-20°C impact)
S355K2 (Enhanced -20°C toughness)
S355N/NL (Normalized, improved low-temp properties)
Mechanical Properties
| Property | S355JR | S355J2 | S355N |
|---|---|---|---|
| Yield Strength (ReH) | ≥355 MPa | ≥355 MPa | ≥355 MPa |
| Tensile Strength (Rm) | 470-630 MPa | 470-630 MPa | 470-630 MPa |
| Elongation (A₅) | ≥22% | ≥22% | ≥22% |
| Impact Energy (KV) | ≥27J @ +20°C | ≥27J @ -20°C | ≥40J @ -50°C |
Chemical Composition (Max %)
| Element | S355JR | S355J2 | Note |
|---|---|---|---|
| C | 0.22 | 0.20 | Lower C improves weldability |
| Si | 0.55 | 0.50 | Deoxidation agent |
| Mn | 1.60 | 1.60 | Strength enhancer |
| P | 0.035 | 0.030 | Reduces cold brittleness |
| S | 0.035 | 0.025 | Improves machinability |
| CEV | ~0.45 | ~0.42 | Carbon Equivalent Value |
Key Features
High Strength: 29% stronger yield strength than S275.
Weldability: Moderate CEV (0.40–0.45); preheat required for thick sections (>30mm).
Corrosion Resistance: Standard grade lacks weathering resistance (use S355J0WP for Corten-like properties).
Processing: Suitable for cutting, bending, and welding (follow EN 1011 guidelines).
Applications
Construction: High-rise buildings, bridges (e.g., Eurocode-compliant designs).
Heavy Equipment: Crane booms, mining machinery.
Transport: Shipbuilding, rail carriages.
Energy: Wind turbine towers (S355NL preferred for low temps).