1. Weldability Fundamentals

Q295GNH: Lower carbon equivalent (Ceq ≈ 0.30–0.35%) due to its lower carbon and alloy content. This gives it better inherent weldability, with lower risk of cold cracking and less sensitivity to heat input.

Q355NH: Higher carbon equivalent (Ceq ≈ 0.38–0.45%) due to increased carbon and alloying elements (e.g., Mn, Cr) to achieve higher strength. This increases its susceptibility to cold cracking and requires stricter control of preheating and heat input.

2. Preheating Requirements

Q295GNH:

Generally requires no preheating for thin sections (<12mm) under normal ambient conditions (above 15°C).

For thicker sections (>12mm) or low-temperature environments (<5°C), preheating to 50–100°C may be recommended to reduce hydrogen-induced cracking.

Q355NH:

Mandatory preheating for most applications, especially for thicknesses >8mm or in cold environments.

Typical preheating temperatures: 80–150°C (higher for thicker plates or high 拘束度 joints to slow cooling and allow hydrogen diffusion).

3. Heat Input Control

Q295GNH: More tolerant of higher heat input. Welding parameters (e.g., current, voltage, travel speed) can be adjusted within a wider range without significant degradation of weld zone toughness.

Recommended heat input: 15–35 kJ/cm (depending on thickness).

Q355NH: Strict heat input limits to avoid grain coarsening in the heat-affected zone (HAZ), which reduces toughness.

Recommended heat input: 15–25 kJ/cm (tighter range to prevent excessive HAZ softening or embrittlement).

4. Filler Metal Selection

Q295GNH:

Filler metals matching its weathering properties and strength: e.g., E7018-G (for weathering) or E6013 (for general structural use).

Focus on maintaining corrosion resistance in the weld metal, often requiring fillers with Cu, Cr additions.

Q355NH:

Requires higher-strength fillers to match its base metal strength: e.g., E8018-G (weathering grade) or E71T-8 (flux-cored, for higher strength).

Critical to balance strength and toughness in the weld, as under-matched fillers may lead to premature failure in the weld zone.

5. Post-Weld Heat Treatment (PWHT)

Q295GNH: Rarely requires PWHT, as its lower alloy content minimizes residual stresses. PWHT may be used only for thick-section, high 拘束度 joints to relieve stress (temperature: 550–600°C).
Q355NH: More likely to require PWHT for thick plates or complex structures to reduce residual stresses and improve HAZ toughness. Typical temperature: 580–620°C (avoiding temper embrittlement ranges).

6. Cracking Prevention

Q295GNH: Primary concern is hydrogen cracking in thick sections; addressed by low-hydrogen electrodes (e.g., E7018-G) and minimal preheating.

Q355NH: Higher risk of cold cracking due to higher carbon and alloy content. Requires:

Strict hydrogen control (low-hydrogen fillers, dry electrodes).

Adequate preheating and interpass temperature (≥150°C for thick sections).

Post-weld slow cooling (e.g., insulation) to allow hydrogen escape.