Welding procedure of ASTM A588 grade B weathering steel plate

Different from ordinary steel plate, ASTM A588 grade B weathering steel plate has good corrosion resistance. In the acid rain and other bad weather, many buildings began to appear different degrees of corrosion, which not only affects the buildings, but also affects the people inside the buildings. It also brings some security risks. The weathering resistance of ASTM A588 grade B weathering steel plate in construction also slows down the corrosion phenomenon of buildings, and achieves good application effect.

 

1. Weld grooves in ASTM A588 grade B weathering steel plate and stainless steel plate are processed respectively;

 

2. After the dirt around the groove is removed by polishing, the groove of the high-grade steel plate is paired with the groove of the stainless steel plate to form the welding area;

 

3. The non pulsating solder is used to weld the welding area of high ASTM A588 grade B weathering steel plate, and the primer layer is formed in the lower part of the welding area;

 

4. Non pulsating solder is used to cover the upper surface of the welding layer in the welding area to form a coating in the welding area. By welding ASTM A588 grade B weathering steel plate under low current and voltage, the heat of ASTM A588 grade B weathering steel plate is reduced and the weldability of ASTM A588 grade B weathering steel plate is improved.