The difference in composition and performance of S355J2WP+N steel plate and S355J2WP steel plate

S355J2WP+N and S355J2WP are both weathering structural steels designed for enhanced corrosion resistance in atmospheric conditions. The key differences lie in their composition, mechanical properties, and processing:

1. Composition Differences:

Both steels have similar base compositions, but S355J2WP+N undergoes normalizing rolling (indicated by "+N"), which refines the grain structure for better toughness. The typical compositions (EN 10025-5 standard) are nearly identical, but slight variations may exist in microalloying elements like Cu, Cr, Ni, and P for improved corrosion resistance.

Element S355J2WP (Typical) S355J2WP+N (Typical)
C ≤0.12% ≤0.12%
Si ≤0.50% ≤0.50%
Mn 0.50-1.50% 0.50-1.50%
P 0.06-0.15% 0.06-0.15%
S ≤0.030% ≤0.030%
Cu 0.25-0.55% 0.25-0.55%
Cr 0.40-0.80% 0.40-0.80%
Ni ≤0.65% ≤0.65%

2. Mechanical Properties:

The "+N" (normalized) version offers better impact toughness at low temperatures due to grain refinement.

Property S355J2WP S355J2WP+N
Yield Strength (ReH) ≥355 MPa ≥355 MPa
Tensile Strength (Rm) 470-630 MPa 470-630 MPa
Elongation (A₅) ≥20% ≥20%
Impact Toughness (KV) ≥27 J at -20°C ≥27 J at -20°C (often better due to normalized structure)

3. Performance Differences:

S355J2WP+N has improved weldability and toughness due to the normalized structure, making it more suitable for low-temperature applications.

Corrosion resistance is similar in both, as they form a protective patina (rust layer) when exposed to weather.

S355J2WP+N is often preferred for heavy structural applications where better internal integrity is required.