GNEE Steel's SA612 steel plate is a high-strength carbon steel plate specifically engineered for pressure vessel and boiler fabrication in moderate to lower temperature service conditions. It conforms to the ASME SA612 / ASTM A612 pressure vessel quality standards and is widely used in welded pressure equipment due to its excellent mechanical properties and weldability.
Material Overview
SA612 is a full-killed carbon-manganese-silicon (C-Mn-Si) steel, meaning it is fully deoxidized during production to ensure a fine, uniform grain structure and improved toughness - especially important for welded assemblies and low-temperature service.
Key Characteristics

1. High Strength and Toughness
SA612 steel provides high tensile and yield strength, making it suitable for welded pressure vessel components under internal pressure and varying temperatures.
2. Excellent Weldability
Its controlled chemical composition and fine grain structure ensure reliable weldability using common welding processes-ideal for complex vessel fabrication.
3. Moderate to Low Temperature Service
Engineered for moderate and lower temperature conditions, SA612 maintains strong mechanical properties and toughness at these regimes.
4. Pressure Vessel Quality (PVQ)
The material meets pressure vessel quality standards and is routinely used for welded boilers and vessels in petrochemical and energy industries.
Typical Chemical Composition
While exact values can vary slightly by supplier and standardization, SA612 plates typically include:
Carbon (C): ≤ 0.25%
Manganese (Mn): ~1.0–1.5%
Silicon (Si): ~0.15–0.50%
Low levels of P and S
Optional alloying elements (Cu, Ni, Cr, Mo, V) depending on spec and application.

Mechanical Properties

Typical mechanical performance (varies with thickness and heat treatment) includes:
Yield Strength: ≥ ~345 MPa
Tensile Strength: ~560–725 MPa
Good elongation and toughness for reliable pressure containment and fabrication performance.
Applications
SA612 steel plate is widely used in industries that require robust pressure-containing structures, including:
Boiler and pressure vessel fabrication
Industrial storage and processing tanks
Heat exchangers and piping systems
Petrochemical and refining equipment
Moderate to low temperature welded structures
These applications benefit from SA612's combination of strength, weldability, and performance reliability under pressure.

Delivery Conditions
GNEE can supply SA612 plates in various conditions based on project requirements:
As-rolled
Normalized
Normalized and Stress-relieved
Surface treatments, anti-rust coatings, or special packaging can also be added per customer request.
GNEE Steel also supplies a variety of boilers and pressure vessel steel plates, such as A204 Grade B,A515 Grade 70,A537 Class 1,SA387 Grade 11 Class 1,P265GH,S537 Class 2,P355Q,P275N,P355N,P690Q,Q345R, etc. If you want to know more about other types of steel plates, you can call the consultation hotline at +8615824687445 or send an email to ru@gneesteelgroup.com. You are welcome to consult us, and we are very willing to answer your questions.
FAQ
What is SA 612 material?
carbon-manganese-silicon steel plate
SA612 is killed carbon-manganese-silicon steel plate made for welded pressure vessels. Its fine grain makes it suitable for use in moderate and lower temperature service where impact resistance is important.
What is the composition of ASTM A612?
ASTM A612 steel plate is a high-strength low-alloy (HSLA) steel plate designed for welded pressure vessels. It has a nominal composition of carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, and copper.
What is A612 steel?
ASTM A612 specification is the Standard Specification for Pressure Vessel Plates, Carbon Steel, High Strength, for Moderate and Lower Temperature Service. ASTM A612 encompasses carbon-manganese-silicon steel plates intended for use in welded pressure vessels for moderate and low temperature service.
Are SA612 and A612 Steel Plates the Same Product? What Are the Core Differences?
They are the same type of steel plate. ASTM A612 is the material standard, while ASME SA612 is the designation assigned after ASTM A612 was incorporated into the ASME Boiler & Pressure Vessel Code, specifically for the fabrication of pressure-bearing equipment.
What Are the Executive Standards for SA612/A612 Steel Plates? Are There Any Differences Between the ASTM and ASME Versions?
The executive standards are ASTM A612/A612M and ASME SA612. There are no substantial differences in chemical composition and mechanical properties between the two versions; the only variance lies in their applicable code systems.
What Are the Equivalent Grades of SA612/A612 in Chinese and European Standards? Can They Be Used as Direct Substitutes?
Common approximate equivalent grades include EN P355GH, DIN 1.0473, and GB Q345R. However, they cannot be used as direct equivalents. Their suitability must be confirmed in accordance with design specifications and approval requirements.
What Are the Yield Strength and Tensile Strength of SA612/A612? Do They Vary with Different Thicknesses?
The minimum yield strength of SA612 is approximately 260 MPa, and its tensile strength ranges from 485–620 MPa. As the thickness increases, the allowable minimum yield strength may decrease slightly.
What Are the Low-Temperature Impact Energy Requirements for SA612/A612? Are the Requirements at -40℃ and -45℃ Consistent?
Standards typically require impact testing at -40℃, while testing at -45℃ is not mandatory. If a project specifies -45℃ testing, additional impact tests must be conducted and clearly defined in the technical agreement.
What Are the Minimum and Maximum Service Temperatures for SA612/A612?
The recommended minimum service temperature is approximately -40℃, and the maximum operating temperature is generally around 400℃, depending on the design specifications and service medium.
What Is the Carbon Equivalent of ASME SA612? Is Preheating Required for Welding?
The carbon equivalent is usually around 0.42–0.45. Preheating at 50–120℃ is recommended for welding medium and thick plates. Commonly used welding materials include low-hydrogen electrodes such as E7018 and E7016.
What Is the Routine Thickness Range of SA612/A612, and What Is the Maximum Customizable Thickness?
The routine thickness range is 6–100 mm. Some steel mills can provide customized thicknesses up to 150 mm, subject to confirmation of their rolling and heat treatment capabilities.
What Are the Common Delivery Conditions for SA612/A612?
Common delivery conditions include As-Rolled (AR), Normalized (N), and Normalized + Tempered (N+T), with the normalized condition being the most widely used.
What Is the Machinability of SA612? Is It Prone to Cracking?
SA612 exhibits excellent cutting and bending performance. When processed with proper techniques and preheating, it is not prone to cracking.
Which Is More Suitable for Low-Temperature Applications: SA612 or SA516 Gr.70?
SA612 delivers more stable comprehensive performance in thick plate and high-stress working conditions, whereas SA516 Gr.70 offers better cost-effectiveness in conventional operating conditions.
Can Q345R Be Used as a Substitute for SA612?
Q345R can be used as a substitute in some working conditions for non-ASME projects. However, substitution is not recommended for export projects or scenarios where SA612 is explicitly required by specifications.
What Are the Differences Between SA612 and SA537 Cl.2?
SA537 Cl.2 boasts higher strength and low-temperature performance but comes with a significantly higher cost than SA612. It is suitable for more severe operating conditions.
Is SA612 Vessel Plate Suitable for LNG Storage Tanks?
SA612 is not recommended for primary LNG storage tanks operating at -162℃, but it can be used in LNG auxiliary systems or medium-to-low temperature vessels.
What Is the Hydrogen-Induced Cracking (HIC) Resistance of SA612 Steel Plates?
Standard SA612 does not mandate HIC resistance requirements. For applications involving sulfur-containing media, customized low-sulfur and low-phosphorus SA612 plates must be used, accompanied by HIC testing.
| Other steel plate by GNEE | ||||
| Name | Material | Specification (mm) | Tons | Remark |
| Clad steel plate | P265GH+410,S355JR+410,A516Gr70+316, A537CL1+304L,Q235B+304L,Q345B+304, A516Gr70(NACE)+410,A537CL1+904L, A537CL1+316L,A516Gr70+304L,A537CL1+304 ,A516Gr70+410,A516Gr70+904L |
2-300mm(Based plate),1-50mm(Composited plate) | / | UT, AR, TMCP.Normalized, Quenched and Tempered,Z Direction Test, Charpy V-Notch impact TestThe Third Party Test , Coated or Shot Blasting and Painting. |
| Low Alloy | Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo | 6 - 350 | 5788.56 | Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection |
| Pressure Vessel Plate | A204 Grade B,A515 Grade 70,A537 Class 1,SA387 Grade 11 Class 1,P265GH,S537 Class 2,P355Q,P275N,P355N,P690Q,Q345R, | 3 - 300 | 8650 | Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection |
| High-Strength Plate | A514 Grade F, A572 Grade 50, A588 Grade A, S355JR, S690Q, SS400, S690QL, Q345B, Q345E | 8 - 120 | 3086.352 | Quenched and tempered |
| Wear-Resistant Plate | NM360, NM400, NM450, NM500 | 6 - 150 | 3866.297 | Quenched and tempered |
| Ship Plate | ABS AH32,ABS DH32,ABS EH32,ABS FH36,ASTM A131 A, ASTM A131 EH32,ASTM A131 AH36,CCS A,CCS AH32,LR AH32, DNV A36,BV AH32 |
8 - 200 | 2853.621 | Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness |