The A242 steel has a yield strength of 50,000 pounds per square inch (340,000 kPa) and ultimate tensile strength of 70,000 psi (480,000 kPa) for light-medium rolled shapes and plates up to 0.75 inches (19 mm) thick. A242 steel has yield strength of 46,000 psi (320,000 kPa) and ultimate strength of 67,000 psi (460,000 kPa) for medium weight rolled shapes and plates from 0.75–1 inch (19–25 mm) thick. The thickest rolled sections and plates – from 1.5–4 in (38–102 mm) thick have yield strength of 42,000 psi (290,000 kPa) and ultimate strength of 63,000 psi (430,000 kPa).
A242 steel Chemical composition in Product analysis
| Grade | Chemical Composition % | Tensile Test | ||||||||
| C | Mn | P | S | Cu | Thickness (t)mm | Yield point ksi(N/mm²) | Tensile strength ksi (N/mm²) | Elongation | ||
| Test piece in(mm) | % min | |||||||||
|
A242 Type1 |
0.15 max | 1.00 max | 0.15 max | 0.05 max | 0.20 min | t≦19.05 | 50(345) min | 70(480) min | GL=8(200) GL=2(50) | 18 21 |
| 19.05<t≦38.10 | 46(315) min | 67(460) min | ||||||||
| 38.10<t≦101.6 | 42(290) min | 63(435) min | ||||||||
Remarks:
1.For plates wider than 24 in.(600mm), the elongation requirement is reduced two percentage points.
2.For nominal thickness under 5/16 in.(8mm), the deduction from the specified percentage of elongation in 8 in.(200mm) shall be made for decreases of the nominal thickness below 5/16 in.(8mm). See elongation requirement adjustments under the Tension Tests section of Specification A6 for deduction values.