+8615824687445
Home / Knowledge / Details

Oct 20, 2025

Are there any specific post-weld treatment requirements for SMA570W?

1. Mandatory Stress Relief Annealing (for High-Stress or Thick Components)

Stress relief annealing is not optional for all SMA570W welds but is required for specific scenarios to prevent delayed cold cracking and stabilize the heat-affected zone (HAZ) microstructure:

Applicable conditions:

Welded components with plate thickness > 20mm (especially load-bearing parts like bridge girders or pressure vessel shells).

Joints subjected to dynamic loads (e.g., seismic activity) or harsh environments (e.g., coastal salt spray).

Process parameters:

Heat the entire welded component uniformly to 550–600°C (avoid exceeding 620°C, which may reduce base metal strength).

Hold at this temperature for 1–2 hours per 25mm of plate thickness (e.g., 4 hours for 50mm-thick plates) to fully release residual stress.

Cool slowly at a rate ≤ 50°C/hour until the component reaches 300°C, then allow air cooling. Rapid cooling will reintroduce stress and risk cracking.

2. Post-Weld Cleaning: Preserve Weathering Performance

SMA570W's corrosion resistance depends on its ability to form a uniform patina, so post-weld cleaning must avoid damaging its surface alloying elements (Cu, Cr):

Remove flux residues and spatter:

Use a wire brush (stainless steel, not carbon steel) or sandblasting (with fine-grain abrasive, e.g., 120-grit) to remove weld spatter and flux slag. Do not use acidic cleaners (e.g., hydrochloric acid) or wire brushes made of ordinary steel-they will corrode the base metal and contaminate the surface.

For hard-to-reach areas (e.g., lap joints), wipe with a cloth dipped in neutral detergent (e.g., pH 6–8) followed by clean water rinsing.

Avoid over-grinding:

 

Only grind to remove surface defects (e.g., shallow cracks or excessive spatter), not for cosmetic purposes. Over-grinding exposes fresh metal without weathering elements, leading to localized rusting that disrupts the patina. If grinding is needed, use a fine-grit 砂轮 (≥ 120 grit) and keep the grinding depth ≤ 0.5mm.

3. Optional Supplementary Treatments (for Extreme Environments)

In ultra-harsh conditions (e.g., offshore platforms or heavy industrial zones), additional treatments can further enhance joint durability-though these are not universal requirements:

Zinc-rich primer touch-up:

 

If the weld surface or heat-affected zone (HAZ) shows signs of early rust (e.g., orange spots) after cleaning, apply a thin layer of zinc-rich primer (zinc content ≥ 90%). This provides temporary protection until the natural patina forms, without compromising the steel's long-term weathering performance.Low-temperature tempering (for thick plates):

 

For plates > 30mm thick, a low-temperature tempering (180–220°C for 2 hours) after stress relief can further refine the HAZ microstructure, improving toughness without reducing strength. This is especially useful for components used in cold regions (below 0°C).

4. Prohibited Post-Weld Practices

Certain treatments will damage SMA570W's properties and must be avoided:

Do not perform "hot peening" (hammering the weld while hot)-this can introduce microcracks in the HAZ and disrupt the patina.

Do not apply ordinary paint (e.g., alkyd paint) as a post-weld coating-this blocks the atmosphere from reacting with the steel, preventing the formation of the protective patina. Only use weathering steel-specific coatings (e.g., transparent acrylic sealants) if required by design.