1. Welding Consumable Selection: Match Toughness and Weather Resistance

Low-temperature toughness: Choose low-hydrogen electrodes/fillers (e.g., E5515-G for SMAW, ER55-G for GMAW) with Charpy V-notch impact values exceeding the base metal's requirements at the service temperature (e.g., ≥27J at -20°C or higher for colder environments). This ensures weld metal and HAZ retain ductility to resist brittle failure.

Weather resistance: Prioritize consumables with alloying elements (Cu, Cr) matching Q460NH to maintain the joint's ability to form a protective, corrosion-resistant patina-critical in low-temperature, high-humidity, or coastal environments where corrosion accelerates.

2. Preheating: Prevent Rapid Cooling and Martensite Formation

Mandatory preheating: Heat the base metal to 100–150°C (measured 50mm from the weld groove) before welding. This slows the cooling rate of the weld and HAZ, preventing the formation of hard, brittle martensite (a microstructure prone to cracking in low temperatures).

Adjust for thickness: For plates thicker than 25mm, increase preheat to 150–200°C to ensure uniform heating through the section, reducing thermal gradients that cause residual stress.

3. Heat Input and Interpass Temperature Control

Limit heat input: Restrict heat input to 20–35kJ/cm to avoid excessive grain growth in the HAZ. Coarse grains in the HAZ drastically reduce low-temperature toughness, making the joint vulnerable to fracture under load.

Control interpass temperature: Maintain it between 150–250°C (never exceeding 250°C). Overheating softens the HAZ and weakens the weathering alloy distribution, impairing both strength and corrosion resistance.

4. Welding Technique: Minimize Stress and Defects

Avoid cold starts/stops: Ensure stable arc initiation and termination to prevent porosity or incomplete fusion-common "crack starters" in low temperatures. Use backstepping or weave techniques for thick sections to distribute heat evenly.

Reduce restraint: Design joints to allow slight expansion/contraction during cooling (e.g., use temporary spacers) to minimize residual stress, which exacerbates brittle fracture risk in cold conditions.

5. Post-Weld Treatment: Relieve Stress and Preserve Integrity

Slow, natural cooling: Never force-cool welds (e.g., with water sprays). Allow joints to cool gradually to ≤50°C to reduce thermal stress and avoid hydrogen trapping (a cause of delayed cracking).

Stress relief annealing: For critical components (e.g., load-bearing joints), perform annealing at 550–620°C for 1–2 hours, then cool slowly. This releases residual stresses that could concentrate and cause failure in low-temperature service.

6. Rigorous Inspection: Validate Low-Temperature Performance

Low-temperature impact testing: Test weld metal and HAZ specimens at the minimum service temperature (e.g., -20°C or -30°C) to confirm Charpy toughness meets specifications.

Non-destructive testing (NDT): Use ultrasonic testing (UT) to detect internal cracks in thick sections and magnetic particle testing (MT) to check for surface flaws in high-stress areas-both critical for identifying hidden defects that may fail in cold environments.