ABS AH32,DH32,EH32,FH32 ABS Grade A/B/D/E,ABS steel plate
GNEE STEEL has many years experience in shipbuilding steel plate, especial in super thickness ship steel plate of ABS AH32, DH32, EH32, FH32, ABS Grade A/B/D/E.
1. Steel Grade : ABS Grade A, ABS Grade B, ABS Grade D,ABS Grade E, ABS AH32, ABS AH36, ABS AH40, ABS DH32, ABS DH36, ABS DH40, ABS EH32, ABS EH36, ABS EH40 ,ABS FH32,ABS FH36,ABS FH40.
2. Dimension(T*W*L) : Thickness:4mm to 300mm ; Width: 1500mm to 4020mm ; Length: 4000mm to 18000mm
3. Adopt Standard: ABS Classification Society.
4. Heat Treatment:
Hot Rolled, CR, Normalized, Quenched, Tempering, TMCP, Electroslag Remelting Technical.
5. Delivery Time: 30-40days
6. Payment Item: 30% TT, or LC and TT.
7. Trade Terms: FOB, CFR, CIF
8. Steel Services: Cutting, Painting, Ball blast, Pretreatment, and The third party inspection in DNV, BV, LR, GL, ABS and CCS in super thick ship steel plate.
ABS Grade AH32 Shipbuilding Steel Plate Chemical Composition and Mechanical Property
| C max | Si max | Mn | P max | S max | Als | Nb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. | N max. |
|
0.18 |
0.50 | 0.90-1.60 |
0.030 |
0.030 |
0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |
- |
| Yield Strength (MPa) min. | Tensile Strength (MPa) | Elongation min. % |
| 315 | 450-570 | 22 |
ABS Grade DH32 Shipbuilding Steel Plate Chemical Composition and Mechanical Property
| C max | Si max | Mn | P max | S max | Als | Nb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. | N max. |
|
0.18 |
0.50 | 0.90-1.60 |
0.025 |
0.0.25 |
0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |
- |
| Yield Strength (MPa) min. | Tensile Strength (MPa) | Elongation min. % |
| 315 | 450-570 | 22 |
ABS Grade EH32 Shipbuilding Steel Plate Chemical Composition and Mechanical Property
| C max | Si max | Mn | P max | S max | Als | Nb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. | N max. |
|
0.18 |
0.50 | 0.90-1.60 |
0.025 |
0.025 |
0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |
- |
| Yield Strength (MPa) min. | Tensile Strength (MPa) | Elongation min. % |
| 315 | 450-570 | 22 |
ABS Grade FH32 Shipbuilding Steel Plate Chemical Composition and Mechanical Property
| C max | Si max | Mn | P max | S max | Als | Nb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. | N max. |
|
0.16 |
0.50 | 0.90-1.60 |
0.020 |
0.0.20 |
0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.80 | 0.08 |
0.009 |
| Yield Strength (MPa) min. | Tensile Strength (MPa) | Elongation min. % |
| 315 | 450-570 | 22 |
GNEE Customer Site Visit

GNEE TEAM

GNEE Customer Office Visit

GNEE Exhibition

GNEE Sales Team

Hot Tags: ABS Grade AH32 DH32 EH32 FH32 Shipbuilding Steel Plate, China ABS Grade AH32 DH32 EH32 FH32 Shipbuilding Steel Plate manufacturers, suppliers, factory